66 2 4 6 1 0 0 0 5 95 95 99 99 0 Tensile strength vs. Temperature for Alloy 800H tube (NRIM/CDS/No.26) fC-UTS X = Test Temperature (¡C) * 1/500 Y = LOG10(UTS) (10X,F6.1,33X,F5.1) 1 3 0.002 0.0